Cathode strips are attained in the dismantled batteries, then soaked in NMP, and go through sonication to get rid of surplus deposits. It really is treated hydrothermally with a solution containing LiOH/Li2SO4 in advance of annealing.[257] Electricity losses arising from electrical contact resist